锰系铁合金的冶炼和用途
高碳锰铁冶炼工艺(熔剂法)冶炼原理: 间接还原 FeO + CO = Fe + CO2 △G°=-49324+40.13T MnO + CO = Mn + CO2 △G°=-412664
+172.16T T始=1229 K (956℃) T始=2396 K (2123℃)
直接还原
MnO + C = Mn + CO △G°=575266-339.78T T始=1693 K 2MnO + 8/3C = 2/3Mn + 2CO △G°=510789.6-340.8T T始=1499 K (软熔带)11